Catalyst
A catalyst for curing Lamit 109 polyester resin and in Lamit lamination kit.
A catalyst for curing Lamit 109 polyester resin and in Lamit lamination kit.
A laminating kit developed for repairs of various laminated parts, e.g. boat hulls, swimming pools and garden ponds, sporting articles, body panels on vehicles, etc.
Laminating polyester preparation: To the required quantity of polyester add during permanent stirring 2% of catalyst. Prepare only such amount of resin that is workable during 15 minutes at temperature +20 °C. Never laminate at temperatures lower than +15 °C. Hardening lasts longer and repair quality decreases.
An all-purpose polyester resin formulated for laminating. Used for laminated parts repairs (boat hulls, swimming pools, etc.) an also for production of laminates based on continuous laminating, winding or injecting. Also for production of agglomerated natural stone slabs and structured stones.